Non-destructive testing of industrial structures with the use of multi-camera digital image correlation method M Malesa, K Malowany, J Pawlicki, M Kujawinska, P Skrzypczak, ... Engineering Failure Analysis 69, 122-134, 2016 | 47 | 2016 |
Corrosion and stress-corrosion cracking of exploited storage tank steel A Zagórski, H Matysiak, O Tsyrulnyk, O Zvirko, H Nykyforchyn, ... Materials Science 40, 421-427, 2004 | 41 | 2004 |
On-line laser triangulation scanner for wood logs surface geometry measurement P Siekański, K Magda, K Malowany, J Rutkiewicz, A Styk, J Krzesłowski, ... Sensors 19 (5), 1074, 2019 | 37 | 2019 |
Creep of degraded 2.25 Cr-Mo steel in hydrogen LO Babii, OZ Student, A Zagórski, AD Markov Materials science 43, 701-707, 2007 | 18 | 2007 |
Nitrogen as an alloying element improving material properties of the high carbon cast steel for ball mill liner plates J Gawlik, J Schmidt, T Nowak, Z Wójcicki, A Zagórski Archives of Civil and Mechanical Engineering 17 (4), 926-934, 2017 | 17 | 2017 |
Corrosion and electrochemical properties of the steel of exploited oil tanks in bottom water O Zvirko, A Zagórski Materials Science 44 (1), 126-132, 2008 | 10 | 2008 |
Tightness and material aspects of bolted flange connections with gaskets of nonlinear properties exposed to variable loads R Walczak, J Pawlicki, A Zagórski Archives of Metallurgy and Materials 61, 2016 | 8 | 2016 |
Ocena rozwoju procesów zmeczeniowych związanych z lokalnymi odksztalceniami na przykładzie stali P91 dla energetyki D Kukla, A Zagórski, P Grzywna Energetyka, 436-440, 2012 | 7 | 2012 |
Ocena rozwoju uszkodzenia zmęczeniowego warstwy aluminidkowej na stopie niklu z zastosowaniem technik nieniszczących D Kukla, A Zagórski Welding Technology Review 87 (12), 2015 | 5 | 2015 |
Effect of the 2, 25Cr-Mo-V steel degradation in service conditions on its creep in hydrogen L Babij, A Zagórski, O Student Фіз.-хім. механіка матеріалів.–2006.–Спецвипуск, 227-232, 2006 | 5 | 2006 |
Creep fracture strength in hydrogen of Cr–Mo–V steel OZ Student, H Matysiak, A Zagórski, LO Babiy, KJ Kurzydłowski Inżyn. Powier 1, 175-179, 2005 | 5 | 2005 |
Mechanical and physical properties of nano-metals M Lewandowska, A Zagorski, KJ Kurzydlowski Materials science forum 654, 1110-1113, 2010 | 4 | 2010 |
Peculiarities of hydrogen effect on the creep process in the Cr-Ni-Mo steel A Zagórski, O Student, L Babij, H Nykyforchyn, KJ Kurzydłowski Advances in Materials Science 7 (1 (11)), 211-218, 2007 | 4 | 2007 |
Tworzywa konstrukcyjne w technologiach wodorowych K Lublińska, A Zagórski, W Spychalski, K Kurzydłowski Przemysł Chemiczny 84 (11), 2005 | 4 | 2005 |
Corrosion degradation of oil-storage tank A Zagórski, H Matysiak, Z Słobodian, O Zvirko, H Nykyforchyn, ... Fiz.-Khim. Mekh. Mater, 437-439, 2004 | 4 | 2004 |
Acoustic emission testing of cryogenic pipelines in operating conditions T Lusa, J Płowiec, M Szwed, Ł Sarniak, A Zagórski Advances in Acoustic Emission Technology: Proceedings of the World …, 2017 | 3 | 2017 |
Ocena rozwoju degradacji zmęczeniowej stali P91 na podstawie zmian kąta fazowego sygnału prądowirowego D Kukla, P Grzywna, A Zagórski Welding Technology Review 84 (13), 2012 | 3 | 2012 |
Application of acoustic emissions to technical evaluation of new pressure devices K Paradowski, WL Spychalski, J Plowiec, T Lusa, A Zagorski, ... European Working Group on Acoustic Emission, 2008 | 3 | 2008 |
Współczesne metody inżynierii materiałowej stosowane do badań materiału konstrukcji pracujących w warunkach wysokiego cisnienia K Kurzydłowski, A Zagórski, W Spychalski, Ł Ciupiński Mechanik 74 (11), 2001 | 3 | 2001 |
Hydrogen influence on microstructure, corrosion resistance and mechanical properties of low alloy steel and explosively cladded steel used for hydrogen storage salt caverns M Gloc, M Szwed, A Zagórski, J Mizera Applied Mechanics and Materials 875, 47-52, 2018 | 2 | 2018 |